441R-96: Report on High-Strength Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 441R-96: Report on High-Strength Concrete Columns

Author(s): ACI Committee 441

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 13

Keywords: high-strength concrete

DOI:

Date: 11/25/1996

Abstract:

Note: 441R-96 is only available in PDF format.

This report reviews the state of the knowledge of the behavior of high-strength concrete (HSC) columns. HSC is defined as concrete with compressive strength exceeding 70 MPa (10,000 psi). Research results are used to discuss the effect of cover concrete and parameters related to transverse reinforcement on strength and ductility of HSC columns subjected to concentric load. The behavior of HSC columns subjected to combined axial load and bending moments is discussed. In addition to discussion on flexureal and axial capacity, the report also focuses on seismic performance of HSC columns.




  