372R-97: Design and Construction of Circular Wire and Strand Wrapped Prestressed Concrete Structure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 372R-97: Design and Construction of Circular Wire and Strand Wrapped Prestressed Concrete Structure

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 22

Keywords: circular prestressed structures

DOI:

Date: 5/7/1997

Abstract:

Note: A newer version of this document exists. This document was replaced by 372R-00.

This report provides recommendations for the design and construction of wrapped circular prestressed concrete structures commonly used for liquid and bulk storage. These structures utilize thin cylindrical shells of either concrete or shotcrete. A thin steel diaphragm is incorporated in shotcreted and precast concrete walls. Vertical post- tensioning is incorporated in cast-in-place concrete walls. Recommendations are applicable to circumferential prestressing achieved by wire or strand wrapping. In wrapping, the wire or strand is fully tensioned before placement on the structural core wall. Procedures preventing corrosion of the prestressing elements have been emphasized. The design and construction of dome roofs are also covered.


Product unavailable, please call +1.248.848.3800