363.2R-98: Guide to Quality Control and Testing of High-Strength Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 363.2R-98: Guide to Quality Control and Testing of High-Strength Concrete

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 18

Keywords: High-Strength Concrete

DOI:

Date: 5/5/1998

Abstract:

Note: A newer version of this document exists. This document was replaced by 363.2R-11.

The special quality control and testing needed to measure reliably the strength of specimens of high-strength concrete and to achieve high-strength concrete consistently are discussed. Preconstruction and construction procedures are covered, including planning trial mixtures, preconstruction meetings, batching, placing and testing. The concept of prequalifying suppliers and laboratories is introduced. A method for the evaluation of date is included.