357R-84: Guide for the Design and Construction of Fixed Offshore Concrete Structures (Reapproved 1997)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 357R-84: Guide for the Design and Construction of Fixed Offshore Concrete Structures (Reapproved 1997)

Author(s): ACI Committee 357

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 26

Keywords: offshore structures

DOI:

Date: 1/1/1984

Abstract:
The report provides a guide for the design and construction of fixed reinforced and/or prestressed concrete structures for service in a marine environment. Only fixed structures which are founded on the seabed and obtain their stability from the vertical forces of gravity are covered. Contents include: materials and durability; dead, deformation, live environmental, and accidental loads; design and analysis; foundations; construction and installation; and inspection and repair. Two appendices discuss environmental loads such as wave, wind, and ice loads in detail, and the design of offshore concrete structures for earthquake resistance.




  