352.1R-89: Recommendations for Design of Slab-Column Connections in Monolithic Reinforced Concrete (Reapproved 1997)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 352.1R-89: Recommendations for Design of Slab-Column Connections in Monolithic Reinforced Concrete (Reapproved 1997)

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 22

Keywords: column connections

DOI:

Date: 1/1/1988

Abstract:

Note: A newer version of this document exists. This document was replaced by 352.1R-11.

Gives recommendations for determining proportions and details of slab-column connections. Includes recommendations for appropriate uses and for determining design forces and strength. Presents design examples.