Title:
Bridging Classical FRC & AASHTO T-397
Author(s):
Manuel Bermudez
Publication:
Web Session
Volume:
ws_F25_ManuelBermudez.pdf
Issue:
Appears on pages(s):
Keywords:
DOI:
Date:
4/27/2026
Abstract:
As Ultra-High Performance Concrete (UHPC) technology continues to advance, there is an increasing need for innovative methods to characterize and assess its unique material properties properly. Sometimes conventional testing techniques used for conventional concrete and FRCs are inaccurate for UHPC, leading to potential discrepancies in the performance assessment of the material. This session will focus on novel approaches tailored specifically for UHPC characterization, highlighting advancements that address the current challenges and improve testing accuracy. Experts from national and international research groups, material suppliers, and industry professionals will present the latest methods for UHPC testing of mechanical properties such as compression and tension, fresh properties, and durability. The session aims to provide essential insights into UHPC material characterization, contribute to design practices, and ultimately improve the longevity and reliability of UHPC applications.