The Use of Thermal Breaks in Balcony Slabs for Energy Efficient Precast Buildings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Use of Thermal Breaks in Balcony Slabs for Energy Efficient Precast Buildings

Author(s): Amir Fam

Publication: Web Session

Volume: ws_F25_AmirFam.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/26/2025

Abstract:
As the global construction industry increasingly turns to prefabricated concrete systems for efficiency, sustainability, and resilience, new challenges and opportunities are emerging, especially in seismic, industrial, and marine environments. This International Session brings together leading experts from academia and industry to explore cutting-edge applications of precast concrete in high-demand structural contexts.