Title: Tech Spotlight: Using Resistivity to Assess Concrete Durability

Author(s): Aram Kalousdian

Publication: Concrete International

Volume: 47

Issue: 11

Appears on pages(s): 68-69

Keywords:

DOI: 10.14359/51749282

Date: 11/1/2025

Abstract:
Resistivity can be implemented in quality assurance and quality control operations to assess concrete durability. This article describes a U.S. Department of Transportation Small Business Innovation Research (SBIR) program project Callentis Consulting Group and Penn State University collaborated on to develop a practical device for measuring pore solution resistivity (PSR) and mixture resistivity and to provide direct calculation of formation factor (FF).