Model for corrosion initiation and propagation based on the resistivity

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Model for corrosion initiation and propagation based on the resistivity

Author(s): Carmen Andrade

Publication: Symposium Paper

Volume: 366

Issue:

Appears on pages(s): 156-169

Keywords: model, service-lie, corrosion, initiation, propagation, resistivity

DOI: 10.14359/51749240

Date: 10/1/2025

Abstract:
Concrete is an efficient material in terms of mechanical strength and functionality, but whose durability is one of present challenges that need particular attention to preserve the reinforcement absent of corrosion during the nominal service life. Present trends on modelling by performance make more complex the quality control testing and lengthens the characterization of new low carbon cement concretes. In present work is presented concrete resistivity as the single parameter able to characterize both corrosion periods through the corresponding mathematical expressions. Resistivity is a non-destructive test which could qualify concrete from its early ages. Based in the relation between diffusivity-corrosion current and resistivity, an integral model based in the resistivity measured at short term in the same specimens than mechanical strength (cured humid), is described. It is also analysed the analogies between the diffusivity and corrosion current and the influence of climate in the resistivity for future challenge of predicting the impact of climatic change.

Related References:

1. Hammond E., Robson Td., 1955, The Engineer January, pp78-80 and 114.115.

2. Monfore G. E., 1968, The electrical resistivity of concrete. Journal PCA, Applied Research Section. May pp. 35

3. Calleja J. 1953, Determination of Setting and Hardening Time of High-Alumina Cements by Electrical Resistance Techniques. Journal of ACI, vol 50 issue 11 pp249

4. Gjorv O. E., Vennesland O., & El-Busaidy A. H.,1987, Diffusion of dissolved oxygen through concrete. Mater. Performance 25(12) pp 39-44

5. Page C.L., Treadaway K.W.J., 1982, Aspects of the electrochemistry of steel in concrete. Nature 297 No. 5862, 109-115

6. Gouda V. K., Monfore, G. E., 1965, A rapid method for studying corrosion inhibition of steel in concrete. Journal of PCA, vol 7 no.3, Sep. pp. 24.

7. Andrade, C. and Gónzalez, J.A., 1978, Quantitative measurements of corrosion rate of reinforcing steels embedded in concrete using polarization resistance measurements. Werkstoffe und Korrosion 29, pp. 515.

8. González J.A., Algaba S., Andrade C., 1980, Corrosion of reinforcing bars in carbonated concrete. British Corrosion Journal, 3, pp.135-139.

9. Andrade C., Fullea J., Alonso C., 2000, The use of the graph corrosion rate-resistivity in the measurement of the corrosion current- Proceedings of the International Workshop on “Measurement and interpretation of the on-site corrosion rate-. MESINA- RILEM Proc. No. 18. Ed. C. Andrade, C. Alonso, J. Fullea, J. Polimon and J. Rodriguez. Rilem Publications S.A.R.L. pp. 157-166.

10. Page, C.L., Lambert, P., Vassie, P.R.W., 1991, Investigations of reinforcement corrosion, 2: Electrochemical monitoring of steel in chloride-contaminated concrete. Materials & Structures, 24, pp. 351-358.

11. McCarter, W. J., and Garvin, S., 1989, Dependence of Electrical Impedance of Cement-Based Materials on their Moisture Condition. J. Phys. D: Appl. Phys., Vol. 22, pp. 1773 – 6.

12. Garboczi E.J. 1990. Permeability, diffusivity, and microstructural parameters: A critical review. Cement and Concrete Research, 20, (4), 591-601.

13. Andrade C., 1993, Calculation of chloride diffusion coefficients in concrete from ionic migration measurements. Cement and Concrete Res., 23, pp. 724-742.

14. Tang, L., 1996, Electrically accelerated methods for determining chloride diffusivity in concrete—current development. Magazine of concrete research, 48(176), 173-179.

15. Andrade. C., Alonso C., Goñi S., 1993, Possibilities for electrical resistivity to universally characterize mass transport processes in Concrete. Proceedings International Conference “Concrete 2000. Economic and durable construction through excellence”. Dundee, UK, Sep pp 1639-1653. Dhir R.K. and jones R. Editors. University of Dundee Pub.

16. Andrade C., Bolzoni F., Fullea J., 2011, Analysis of the relation between water and resistivity isotherms in concrete. Materials and Corrosion, 62, no.2, pp. 130-138.

17. Andrade, C., 2004, Calculation of initiation and propagation periods of service-life of reinforcements by using the electrical resistivity. International Symposium on Advances in Concrete through Science and Eng., RILEM Symposium, March, pp. 22-24, Evanston (Illinois, USA).

18. Archie, G.E., 1942, “The electrical resistivity log as an aid in determining some reservoir characteristics” AIME Trans. 146, 54.

19. Wenner, F., 1915, A method of measuring earth resistivity. Bureau of Standards, Bull. 12((4) 258): p. 478-496.

20. EN 12398-19 Testing of hardened concrete. Determination of electrical resistivity. - Part 19: Determination of resistivity

21. Morris W., Moreno E.I., Sagüés A.A., 1996, Practical evaluation of resistivity of concrete in test cylinders using a Wenner array probe, Cement and Concrete Research, 26, pp. 1779-1787.

22. Andrade C., Zuloaga P., Martinez I., Castillo A., Briz S., 2011, Effect of temperature on the corrosion parameters and apparent activation energy measured by embedded sensors in a pilot container in “El Cabril” repository. Corrosion Engineering, Science and Technology. Vol 46 No 2, pp 182-189.

23. Andrade C. Whiting D., 1995, Comparison of AASHTO T-277 (Electrical) and AASHTO T-257 (90d ponding) results. Proceedings 1st RILEM workshop on Chloride Penetration into Concrete 15-18 october, St Rémy lès Chevreuse, France

24. ASTM C1202-22e1 -Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration

25. Andrade, C., d’Andrea R., and Rebolledo N., 2014, Chloride ion penetration in concrete: The reaction factor in the electrical resistivity model, Cement and Concrete Composites, 47, pp. 41-46.

26. Andrade C., Castellote M., D’Andrea R., 2011, Measurement of ageing effect of chloride diffusion coefficients in cementitious matrices. Journal of Nuclear Materials, 412, pp. 209-216.

27. Andrade C., d`Andréa R., 2010, Concrete mix design based on the electrical resistivity. 2nd International Conference on Sustainable Construction Materials and Technologies. Ancona- Italy June. Ed. Coventry University UK.