Notable Concrete in Baltimore

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Notable Concrete in Baltimore

Author(s):

Publication: Concrete International

Volume: 47

Issue: 10

Appears on pages(s): 39-44

Keywords:

DOI: 10.14359/51749206

Date: 10/1/2025

Abstract:
The concrete community will gather for the ACI Concrete Convention from October 26 to 29, 2025, in Baltimore, MD, USA. ACI Concrete Conventions provide an opportunity to consider the contributions of local chapter members and others to outstanding concrete projects. Notable projects in Baltimore include Avalon Harbor East/Avalon 555 President, Elan Brewers Hill, Exelon Tower-Base Building, I-895 Bridge Project, Liberty Harbor East, and the restoration of Recreation Pier.




  