Strength Development and Neutralization Progress in High-Performance Blended Cement Concrete Exposed to Atmospheric, Tidal, and Submerged Sea Conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength Development and Neutralization Progress in High-Performance Blended Cement Concrete Exposed to Atmospheric, Tidal, and Submerged Sea Conditions

Author(s): Hyeong-Ki Kim, Jong-Suk Lee, Hyeon-Woo Lee and Seung-Jun Kwon

Publication: IJCSM

Volume: 19

Issue:

Appears on pages(s):

Keywords: High-performance concrete, Exposure condition, Seawater, Neutralization, Strength development, Code

DOI: 10.1186/s40069-025-00788-y

Date: 9/30/2025

Abstract:
This study investigates the strength development and neutralization depth of high-performance concrete exposed to marine conditions for 7 years on the East coast of South Korea. Blended cements, common in coastal structures, were used. OPC and slag cement showed advantages in strength development, while high-volume fly ash concrete exhibited a disadvantage, especially in external exposure conditions. Despite exposure differences, all mixtures demonstrated a substantial strength increase at 7 years compared to the 28-day period. Models, initially validated for normal-strength concrete, proved effective in predicting long-term behavior. Neutralization depth remained consistent across exposure conditions, with slag cement showing resilience, while fly ash increased depth. Considerations for marine concrete design and construction are discussed.