Shear Creep Failures of Reinforced Concrete Slender Beams without Shear Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Creep Failures of Reinforced Concrete Slender Beams without Shear Reinforcement

Author(s): H. Alfisa Saifullah, K. Nakarai, V. Piseth, N. Chijiwa, and K. Maekawa

Publication: Structural Journal

Volume: 114

Issue: 6

Appears on pages(s): 1581-1590

Keywords: creep; experiment; loading rate; shear strength; sustained load.

DOI: 10.14359/51749187

Date: 11/1/2017

Abstract:
This study aims at investigating the effects of sustained loads on the shear strengths of reinforced concrete (RC) slender beams. Slow loading rates (that were 100 and 1000 times slower than the normal loading rate) were selected to reveal creep effects. The slower loading rate indicated that increased creep occurred during the loading test. However, the shear strength was almost constant during the occurrence of significant diagonal cracking and it increased slightly at failure. It showed that a reduction factor for the shear strengths of the slender RC beams under sustained loads was not required in the design.

Related References:

1. Price, W. H., “Factors Influencing Concrete Strength,” ACI Journal Proceedings, V. 47, No. 2, Feb. 1951, pp. 417-432.

2. Rusch, H., “Researches Toward a General Flexural Theory for Structural Concrete,” ACI Journal Proceedings, V. 57, No. 7, July 1960, pp. 1-28.

3. Rossi, P.; Godart, N.; Robert, J. L.; Gervais, J. P.; and Bruhat, D., “Investigation of the Basic Creep of Concrete by Acoustic Emission,” Materials and Structures, V. 27, No. 9, 1994, pp. 510-514. doi: 10.1007/BF02473211

4. Tasevski, D.; Ruiz, M.; and Muttoni A., “Analogy between Sustained Loading and Strain Rate Effects on the Nonlinear Creep Response of Concrete,” CONCREEP 10, American Society of Civil Engineers, Austria, 2015, pp. 1187-1193.

5. Fu, H.; Erki, M.; and Seckin, M., “Review of Effects of Loading Rate on Concrete in Compression,” Journal of Structural Engineering, ASCE, V. 117, No. 12, 1991, pp. 3645-3659. doi: 10.1061/(ASCE)0733-9445(1991)117:12(3645)

6. Wittmann, F. H.; Roelfstra, P. E.; Mihashi, H.; Huang, Y.-Y.; Zhang, X.-H.; and Nomura, N., “Influence of Age of Loading, Water-Cement Ratio and Rate of Loading on Fracture Energy of Concrete,” Materials and Structures, V. 20, No. 2, 1987, pp. 103-110. doi: 10.1007/BF02472745

7. Wu, S.; Chen, X.; and Zhou, J., “Influence of Strain Rate and Water Content on Mechanical Behavior of Dam Concrete,” Construction and Building Materials, V. 36, 2012, pp. 448-457. doi: 10.1016/j.conbuildmat.2012.06.046

8. Fluck, P. G., and Washa, G. W., “Creep of Plain and Reinforced Concrete,” ACI Journal Proceedings, V. 54, No. 4, Apr. 1958, pp. 879-895.

9. Nie, J., and Cai, C., “Deflection of Cracked RC Beams under Sustained Loading,” Journal of Structural Engineering, ASCE, V. 126, No. 6, 2000, pp. 708-716. doi: 10.1061/(ASCE)0733-9445(2000)126:6(708)

10. Choi, W.-C., and Yun, H.-D., “Long-Term Deflection and Flexural Behavior of Reinforced Concrete Beams with Recycled Aggregate,” Materials & Design, V. 51, 2013, pp. 742-750. doi: 10.1016/j.matdes.2013.04.044

11. Adhikary, S. D.; Li, B.; and Kazunori, F., “Effects of High Loading Rate on Reinforced Concrete Beams,” ACI Structural Journal, V. 111, No. 3, May-June 2014, pp. 651-660.

12. Kishi, N.; Mikami, H.; Matsuoka, K. G.; and Ando, T., “Impact Behavior of Shear-Failure-Type RC Beams Without Shear Rebar,” International Journal of Impact Engineering, V. 27, No. 9, 2002, pp. 955-968. doi: 10.1016/S0734-743X(01)00149-X

13. Somraj, A.; Fujikake, K.; and Li, B., “Influence of Loading Rate on Shear Capacity of Reinforced Concrete Beams,” International Journal of Protective Structures, V. 4, No. 4, 2013, pp. 521-543. doi: 10.1260/2041-4196.4.4.521

14. Adhikary, S. D.; Li, B.; and Fujikake, K., “Strength and Behavior in Shear of Reinforced Concrete Deep Beams under Dynamic Loading Conditions,” Nuclear Engineering and Design, V. 259, 2013, pp. 14-28. doi: 10.1016/j.nucengdes.2013.02.016

15. Fu, H.; Erki, M.; and Seckin, M., “Review of Effects of Loading Rate on Reinforced Concrete,” Journal of Structural Engineering, ASCE, V. 117, No. 12, 1991, pp. 3660-3679. doi: 10.1061/(ASCE)0733-9445(1991)117:12(3660)

16. Sarkhosh, R., “Shear Resistance of Reinforced Concrete Beam without Shear Reinforcement under Sustained Loading,” PhD dissertation, Delft University of Technology, Delft, the Netherlands, 2015.

17. Sarkhosh, R.; Walraven, J. C.; Den Uijl, J. A.; and Braam, C. R., “Shear Capacity of Concrete Beams under Sustained Loading,” The 36th Symposium of IABSE, India, 2013, pp. 162-169.

18. Maekawa, K.; Zhu, X.; Chijiwa, N.; and Tanabe, S., “Mechanism of Long-Term Excessive Deformation and Delayed Shear Failure of Underground RC Box Culverts,” Journal of Advanced Concrete Technology, V. 14, No. 5, 2016, pp. 183-204. doi: 10.3151/jact.14.183

19. Piseth, V.; Nakarai, K.; Chijiwa, N.; and Maekawa, K., “Experimental Study on the Effects of a Loading Rate on the Shear Performance of an RC Beam,” CONCREEP 10, American Society of Civil Engineers, Austria, 2015, pp. 1561-1569.

20. Nakarai, K.; Morito, S.; Ehara, M.; and Matsushita, S., “Shear Strength of Reinforced Concrete Beams: Concrete Volumetric Change Effects,” Journal of Advanced Concrete Technology, V. 14, No. 5, 2016, pp. 229-244. doi: 10.3151/jact.14.229

21. Per Johan, G., and Arne, H., “Sensitivity in Shear Strength of Longitudinally Reinforced Concrete Beams to Fracture Energy of Concrete,” ACI Structural Journal, V. 85, No. 3, May-June 1988, pp. 286-294.

22. Sato, R., and Kawakane, H., “A New Concept for the Early Age Shrinkage Effect on Diagonal Cracking Strength of Reinforced HSC Beams,” Journal of Advanced Concrete Technology, V. 6, No. 1, 2008, pp. 45-67. doi: 10.3151/jact.6.45

23. Niwa, J.; Yamada, K.; Yokozawa, K.; and Okamura, H., “Revaluation of the Equation for Shear Strength of Reinforced Concrete Beams Without Web Reinforcement,” Doboku Gakkai Rombunshuu, V. 372, No. 372, 1986, pp. 167-176. doi: 10.2208/jscej.1986.372_167