Title: Field Guide to Placing and Finishing Type IL Cement Concrete

Author(s): Chad White, Bryan M. Birdwell, Jerry A. Holland, and Michael G. Hernandez

Publication: Concrete International

Volume: 47

Issue: 8

Appears on pages(s): 41-45

Keywords: slab, finishing, placement, limestone

DOI: 10.14359/51749080

Date: 8/1/2025

Abstract:
This article discusses differences between ordinary portland cement (Type I/II) and portland-limestone cement (Type IL) concrete based on direct observations and reports from concrete finishers. Developing an understanding of how these two concrete types differ from each other can help contractors modify and adapt finishing practices to avoid possible issues during placement.