Probabilistic Service Life Analysis using Reactive Transport Degradation Modeling

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Probabilistic Service Life Analysis using Reactive Transport Degradation Modeling

Author(s): Cantin

Publication: Web Session

Volume: ws_S25_Cantin.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/30/2025

Abstract:
This presentation will emphasize the role of probabilistic modeling in predicting the service life of concrete structures, focusing on the effects of variability in input parameters like concrete properties, environmental conditions, and cover depth. Through real-world case studies, it will explore the challenges of measuring and validating essential inputs and highlight the significance of sensitivity analyses to identify key factors. Attendees will gain insights into strategies that support more reliable design, maintenance, and rehabilitation decisions for concrete structures.