Evaluating the Shear Strength of Lightweight Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluating the Shear Strength of Lightweight Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bar

Author(s): Karroum

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/30/2025

Abstract:
This research examines the shear strength of lightweight concrete (LWC) beams reinforced with Glass Fiber-Reinforced Polymer (GFRP) bars. It aims to address the current gap in the ACI code regarding the use of GFRP bars in lightweight concrete structures, as existing guidelines primarily focus on normal weight concrete (NWC).