Development and Application of High-Calcium and Phosphate Concrete for Artificial Reef Construction: A Case Study in the Galapagos Islands

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development and Application of High-Calcium and Phosphate Concrete for Artificial Reef Construction: A Case Study in the Galapagos Islands

Author(s): Damaris Jurado

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 12/15/2025

Abstract:
Coral reefs are critical to marine biodiversity yet face severe threats from climate change, pollution, and overexploitation. This research explores the application of concrete made with high calcium and phosphorus content as a material for artificial reef construction, focusing on implementation in the Galápagos Islands.