Title: Sustainable Concrete Mixes using Hypersaline Arabian Gulf Seawater

Author(s): Rahman

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/3/2024

Abstract:
This study covers the replacement of freshwater in concrete with hypersaline seawater, which is used both in blending the concrete mix and curing.