Title: Sustainability, Durability, and Fiber-Reinforced Concrete

Author(s): Beverly Heasley

Publication: Web Session

Volume: ws_F24_Heasley.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/3/2024

Abstract:
In today's 'throw-away culture' it is more important than ever to understand how everyone can contribute to greener, more sustainable, carbon-neutral living. The case studies covered in this presentation show how using fiber-reinforcement in concrete construction plays a key part of the construction industry's role in this effort - from large-scale infrastructure and industrial projects to small business and residential projects.