Title: Slashing Construction Times with Fiber-Reinforced Concrete

Author(s): Deborah R. Huso

Publication: Concrete International

Volume: 47

Issue: 7

Appears on pages(s): 47-50

Keywords: track, slab, steel, bars

DOI: 10.14359/51748937

Date: 7/1/2025

Abstract:
To reduce costs and minimize construction schedules for the recent light rail extension in the Phoenix, AZ, USA metropolitan area, track slabs and platform plinths were constructed using fiber-reinforced concrete instead of traditional steel-reinforced concrete. For every concrete placement, the use of fiber-reinforced concrete is estimated to have saved at least 1 to 2 days of labor.