Title: The Shotcrete Advantage: Enhancing Access, Efficiency, and Safety in Geohazard Mitigation

Author(s): Simon Boone

Publication: Concrete International

Volume: 47

Issue: 7

Appears on pages(s): 30-31

Keywords: stabilization, wall, soil, robot

DOI: 10.14359/51748933

Date: 7/1/2025

Abstract:
In July 2024, GeoStabilization International used shotcrete for the construction of a soil nail wall for a large data center in Atlanta, GA, USA. To enhance efficiency, GeoStabilization implemented innovative techniques, including the use of a shotcrete robot. This proved especially effective during the installation of the initial structural layer of the wall.