Title: Experimental and Analytical Study on Vertical Punching in Flat Plates with Stirrups

Author(s): Srinivas Mogili and Shyh-Jiann Hwang

Publication: Structural Journal

Volume: 123

Issue: 1

Appears on pages(s): 89-104

Keywords: ACI 318; analytical; design codes; flat plates; punching; reinforced concrete; shear strength; softened strut-and-tie (SST) model; stirrups

DOI: 10.14359/51748929

Date: 1/1/2026

Abstract:
Brittle punching failures in flat plates are precluded by ensuring adequate shear strength. Typically, this is achieved by adding shear reinforcement in the design. This paper presents an experimental and analytical study of flat plates to investigate load-resisting mechanisms associated with stirrup addition. The experimental program includes four isolated flat plates with parametric variations tested under monotonic punching loads. In terms of normalized shear strength, improvements of 22% and 29% were observed in flat plates with different layouts of stirrups, respectively, when compared with the reference specimen without stirrups. The role of longitudinal and shear reinforcements in punching resistance of flat plates was assessed through strain observations. Based on test findings, a physics-based analytical procedure for punching capacity estimation is proposed and verified using a database of 72 isolated flat-plate specimens. The proposed method provided reasonably accurate capacity estimates with an overall mean test-to-estimated capacity ratio of 1.06 and a low coefficient of variation (COV) of 13%. These estimates are also compared with capacity predictions using ACI 318-19 guidelines, which resulted in an overall mean capacity ratio of 1.58 with a COV of 22%. Based on experimental and analytical results, modifications to ACI 318-19 two-way shear provisions are suggested by incorporating the key parameters in shear strength estimations, which improved the prediction accuracy to a mean of 1.25 with a COV of 13%.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

2. Mogili, S.; Lin, H.-Y.; and Hwang, S.-J., “Vertical Punching Capacity of Reinforced Concrete Flat Plates without Shear Reinforcement,” ACI Structural Journal, V. 121, No. 1, Jan. 2024, pp. 171-184.

3. Vollum, R. L.; Abdel-Fattah, T.; Eder, M.; and Elghazouli, A. Y., “Design of ACI-Type Punching Shear Reinforcement to Eurocode 2,” Magazine of Concrete Research, V. 62, No. 1, 2010, pp. 3-16.

4. Broms, C. E., “Shear Reinforcement for Deflection Ductility of Flat Plates,” ACI Structural Journal, V. 87, No. 6, Nov.-Dec. 1990, pp. 696-705.

5. Yamada, T.; Nanni, A.; and Endo, K., “Punching Shear Resistance of Flat Slabs: Influence of Reinforcement Type and Ratio,” ACI Structural Journal, V. 88, No. 4, Sept.-Oct. 1992, pp. 555-563.

6. Lips, S.; Fernández Ruiz, M.; and Muttoni, A., “Experimental Investigation on Punching Strength and Deformation Capacity of Shear-Reinforced Slabs,” ACI Structural Journal, V. 109, No. 6, Nov.-Dec. 2012, pp. 889-900.

7. Schmidt, P.; Kueres, D.; and Hegger, J., “Punching Shear Behavior of Reinforced Concrete Flat Slabs with a Varying Amount of Shear Reinforcement,” Structural Concrete, V. 21, No. 1, 2020, pp. 235-246.

8. Oliveira, D. R.; Melo, G. S.; and Regan, P. E., “Punching Strengths of Flat Plates with Vertical or Inclined Stirrups,” ACI Structural Journal, V. 97, No. 3, May-June 2000, pp. 485-491.

9. Hwang, S.-J., and Lee, H.-J., “Strength Prediction for Discontinuity Regions by Softened Strut-and-Tie Model,” Journal of Structural Engineering, ASCE, V. 128, No. 12, 2002, pp. 1519-1526.

10. Hwang, S.-J.; Tsai, R.-J.; Lam, W.-K.; and Moehle, J. P., “Simplification of Softened Strut-and-Tie Model for Strength Prediction of Discontinuity Regions,” ACI Structural Journal, V. 114, No. 5, Sept.-Oct. 2017, pp. 1239-1247.

11. Mogili, S., and Hwang, S.-J., “Softened Strut-and-Tie Model for Shear and Flexural Strengths of Reinforced Concrete Pile Caps,” Journal of Structural Engineering, ASCE, V. 147, No. 11, 2021, p. 04021169.

12. Thürlimann, B., “Shear Strength of Reinforced and Prestressed Concrete–CEB Approach,” Concrete Design: U.S. and European Practices: ACI-CEB-PCI-FIP Symposium, SP-59, American Concrete Institute, Farmington Hills, MI, 1979, pp. 93-115.

13. Rankin, G. I. B., and Long, A. E., “Predicting the Punching Strength of Conventional Slab-Column Specimens,” Proceedings of the Institution of Civil Engineers, V. 82, No. 2, 1987, pp. 327-346.

14. Chana, P. S., and Desai, S. B., “Design of Shear Reinforcement Against Punching,” The Structural Engineer, V. 70, No. 9, 1992, pp. 159-164.

15. Hassan, M.; Abdel Rahman, A.; Sherif, A.; Osman, M.; and Ahmed, A., “Pilot Experimental Tests on Punching Shear Strength of Flat Plates Reinforced with Stirrups Punching Shear Reinforcement,” Journal of Materials and Engineering Structures, V. 4, No. 1, 2017, pp. 3-10.

16. Hegger, J.; Sherif, A. G.; Kueres, D.; and Siburg, C., “Efficiency of Various Punching Shear Reinforcement Systems for Flat Slabs,” ACI Structural Journal, V. 114, No. 3, May-June 2017, pp. 631-642.

17. Mabrouk, R. T. S.; Bakr, A.; and Abdalla, H., “Effect of Flexural and Shear Reinforcement on the Punching Behavior of Reinforced Concrete Flat Slabs,” Alexandria Engineering Journal, V. 56, No. 4, 2017, pp. 591-599.

18. Nayef, S.; Zaki, W.; and Rabie, M., “Effect of Reinforcement on Punching Shear Behavior of Flat Slabs,” International Journal of Civil Engineering and Technology (IJCIET), V. 10, No. 2, 2019, pp. 2403-2418.

19. Regan, P. E., and Samadian, F., “Shear Reinforcement Against Punching in Reinforced Concrete Flat Slabs,” The Structural Engineer, V. 79, No. 10, 2001, pp. 24-31.

20. Marzouk, H., and Hussein, A., “Experimental Investigation on the Behavior of High-Strength Concrete Slabs,” ACI Structural Journal, V. 88, No. 6, Nov.-Dec. 1991, pp. 701-713.

21. Bažant, Z. P., and Yu, Q., “Reliability, Brittleness, Covert Understrength Factors, and Fringe Formulas in Concrete Design Codes,” Journal of Structural Engineering, ASCE, V. 132, No. 1, 2006, pp. 3-12.

22. Bažant, Z. P.; Yu, Q.; Gerstle, W.; Hanson, J.; and Ju, J. W., “Justification of ACI 446 Proposal for Updating ACI Code Provisions for Shear Design of Reinforced Concrete Beams,” ACI Structural Journal, V. 104, No. 5, Sept.-Oct. 2007, pp. 601-610.


ALSO AVAILABLE IN:

Electronic Structural Journal