Integrating 3D Modeling and Non-Linear Numerical Simulations in Concrete Additive Manufacturing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Integrating 3D Modeling and Non-Linear Numerical Simulations in Concrete Additive Manufacturing

Author(s): Jan Cervenka

Publication: Web Session

Volume: ws_S25_Cervenka.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/30/2025

Abstract:
This session will provide a state-of-the-art review of modeling techniques for 3D printing with concrete (3DPC) that are necessary for designing the printed structure, accounting for material properties and printing process parameters. The session blends contributions on latest research developments, current research trajectories, and practical applications.