Title: Admixtures for LC3 Cements

Author(s): Cesar Constantino

Publication: Web Session

Volume: ws_S25_CesarConstantino.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/30/2025

Abstract:
LC3 cements are being developed in the US and are only in use in other countries. Admixtures specific for the these cements will enable their use to replace higher clinker content cements. This presentation will highlight the differences in these admixtures compared to "typical" admixtures and lower our carbon footprint.