Composite SCC and 3-D-Printed Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Composite SCC and 3-D-Printed Concrete Columns

Author(s): Johan L. Silfwerbrand

Publication: Concrete International

Volume: 47

Issue: 6

Appears on pages(s): 33-37

Keywords: form, load, test, research

DOI:

Date: 6/1/2025

Abstract:
Concrete columns are traditionally produced by placing concrete into a mold or form. Assembling and then removing the formwork takes time and labor; and eventual replacement of the formwork leads to increased material use and transport costs. A new alternative, a permanent three-dimensionally (3-D) printed concrete form in which a core is cast with self-consolidating concrete, was investigated in this project.




  