Title: ACI PRC-130.1-25: Environmental Product Declarations (EPDs) of Cement-Based Products: State of Practice and Path Forward—TechNote

Author(s): ACI Committee 130

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 5

Keywords:

DOI:

Date: 4/1/2025

Abstract:
What are cement-based product Environmental Product Declarations (EPDs) and how are they used to support sustainability-related efforts? Keywords: Environmental Product Declarations (EPDs); life cycle assessment (LCA); sustainability.