Concrete Q&A: Moisture Conditioning of Core Samples

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q&A: Moisture Conditioning of Core Samples

Author(s):

Publication: Concrete International

Volume: 47

Issue: 2

Appears on pages(s): 66-68

Keywords: strength, test, curing, gradient

DOI: 10.14359/51745617

Date: 2/1/2025

Abstract:
Should concrete core samples extracted from a structure be submerged in water until testing? This month’s Q&A provides answer to that question along with a discussion on proper and improper moisture conditioning of cores to be tested per ASTM C42/C42M.

Related References:

1. ASTM C42/C42M-20, “Standard Test Method for Obtaining and Testing Drilled Cores and Sawed Beams of Concrete,” ASTM International, West Conshohocken, PA, 2020, 7 pp.

2. ASTM C39/C39M-21, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2021, 8 pp.

3. ACI Committee 214, “Obtaining Cores and Interpreting Core Compressive Strength Results—Guide (ACI PRC-214.4-21),” American Concrete Institute, Farmington Hills, MI, 2021, 20 pp.