Synergizing Ultra-High-Performance and Conventional Concrete in Composite Sections for Economy and Sustainability

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Synergizing Ultra-High-Performance and Conventional Concrete in Composite Sections for Economy and Sustainability

Author(s): Avinaya Tripathi

Publication: Web Session

Volume: ws_F24_Tripathi.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/3/2024

Abstract:
This presentation explores the composite behavior of ultra high performance concrete (UHPC) printed in conjunction with conventional concrete, and evaluates the flexural response and cracking behavior of the composite system. Digital image correlation to determine crack propagations and a composite model for stress-strain relations are proposed. The talk demonstrates the synergy that can be obtained in developing cost-effective, high-performance cementitious composites using 3D printing.