The Concrete Industry’s Perspective on Public Procurement of Low Carbon Construction Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Concrete Industry’s Perspective on Public Procurement of Low Carbon Construction Materials

Author(s): Brian Killingsworth

Publication: Web Session

Volume: ws_F24_BrianKillingsworth.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/3/2024

Abstract:
Through policy and legislation, public infrastructure owners are beginning to procure construction materials with reduced environmental impact by primarily focusing on global warming potential. These efforts are commendable and coincide with the cement and concrete industry’s efforts to be net zero by 2050. The concrete industry has been a leader in benchmarking it’s environmental footprint and transparently reporting through the development of Environmental Product Declarations for over a decade. This presentation will highlight these efforts and discuss further enhancements made to meet public procurement policies.