Interface Shear Failure Behavior Between Normal Concrete (NC) and Ultra-High Performance Concrete (UHPC)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Interface Shear Failure Behavior Between Normal Concrete (NC) and Ultra-High Performance Concrete (UHPC)

Author(s): Boshan Zhang, Jiangjiang Yu, Weizhen Chen, Jianbo Chen, Heng Li & Jialun Niu

Publication: IJCSM

Volume: 18

Issue:

Appears on pages(s):

Keywords: NC–UHPC interface, Interfacial shear failure, Interface roughness, Microstructure of ITZ (interface transition zone)

DOI: 10.1186/s40069-023-00657-6

Date: 12/31/2024

Abstract:
Ultra-high performance concrete (UHPC) with excellent mechanical properties and durability is a promising material for reinforcement of existing normal concrete (NC) structures. In this paper, the shear failure behavior of the NC–UHPC interface was studied by the slant shear test and the SEM (scanning electron microscope) visualization test, considering influence of the substrate strength and the interface roughed treatment. As the NC substrate and the UHPC overlay are tightly combined at the interface transition zone (ITZ), the interface exhibits good slant shear performance, and the measured interfacial shear strength could reach 19.4 MPa with C40 substrate and 21.8 MPa with C50 substrate. In addition, the microstructure and composition of the ITZ, the possible interfacial failure modes, and the load-carrying mechanism of the interface under compression–shear force are revealed. The high interface roughness and the substrate strength have positive influence on the shear strength, and greatly affect the prone failure mode and the load-slip characteristic.