Enhancing Structural Resilience: Microbial-Based Self-Healing in High-Strength Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Enhancing Structural Resilience: Microbial-Based Self-Healing in High-Strength Concrete

Author(s): Tesfaye Alemu Mohammed, Yonathan Muche Kasie, Eleyas Assefa, Yiglet Mebrat Getu & Dereje Hailu Tufa

Publication: IJCSM

Volume: 18

Issue:

Appears on pages(s):

Keywords: Bacillus flexus, Compressive strength, Concrete durability, High-strength concrete, Microbial self-healing, Sporosarcina koreensis

DOI: 10.1186/s40069-024-00661-4

Date: 5/31/2024

Abstract:
Concrete’s weak tensile strength renders it susceptible to cracking under prolonged loads, leading to reduced load-bearing capacity and reinforcing bar corrosion. This study investigates the effectiveness of microbial-based self-healing in high-strength concrete, focusing on two bacterial strains: Sporosarcina koreensis and Bacillus. Results demonstrate significant enhancements in micro- and macro-physical properties of high-strength bacterial concrete with Bacillus flexus and S. koreensis, surpassing the control. Bacillus flexus-infused concrete exhibits a remarkable 21.8% increase in compressive strength at 7 days and 11.7% at 56 days. Similarly, S. koreensis-treated concrete shows 12.2% and 7.4% increases at 7 and 56 days, respectively. Enhanced crack healing occurs due to calcite precipitation, confirmed by X-ray diffraction and scanning electron microscopy. Both bacterial strains achieve crack closure within 42 days, with widths of 259.7 µm and 288.7 µm, respectively. Moreover, bacterial concrete from these strains excels in durability against water, acid, and salt exposure, surpassing control concrete. These findings emphasize microbial-based self-healing’s potential in high-strength concrete, providing a practical strategy to enhance structural resilience and extend concrete infrastructure lifespan.