ACI PRC-213.1-24: Curing Efficiency of Internally Cured Concrete—TechNote

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI PRC-213.1-24: Curing Efficiency of Internally Cured Concrete—TechNote

Author(s): ACI Committee 213

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 6

Keywords:

DOI:

Date: 12/10/2024

Abstract:
Does internal curing impact the duration of external curing that is needed? If so, how much of a reduction in conventional external curing may be expected when internal curing is used? Keywords: curing compound; curing duration; degree of hydration; internal curing; lightweight aggregates; supplementary cementitious materials; wet burlap curing.