From Global to Local Deformations of Concrete Frame Members Accounting for Steel Properties

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: From Global to Local Deformations of Concrete Frame Members Accounting for Steel Properties

Author(s): Drit Sokoli, Albert Limantono, Duy V. To, Jack P. Moehle, and Wassim M. Ghannoum

Publication: Structural Journal

Volume: 122

Issue: 3

Appears on pages(s): 133-145

Keywords: Grade 100 reinforcement; high-strength reinforcement; plasticity; rotation; special moment frames; strains

DOI: 10.14359/51744380

Date: 5/1/2025

Abstract:
Performance-based seismic standards establish acceptance criteria to determine whether structural members can adequately withstand seismic deformation demands. These criteria primarily consist of member deformation limits, such as plastic rotation. There is, however, a shift towards strain-based limits, as strains can provide more reliable estimates of material damage, strength degradation, and can better account for variations in member boundary conditions such as axial load. The process of estimating local material strains in concrete members remains challenging, mainly due to paucity of physical models and test data at the strain level. To address this challenge, a framework based on fiber-section elements and mechanics-based behavioral models is proposed. This framework allows for strain demand estimates based on member-level deformations. Particularly, the framework provides strain demands on longitudinal bars and concrete within the plastic hinge regions of frame members while accounting for differences in steel properties as grade increases.

Related References:

1. ASCE/SEI 41-17, “Seismic Rehabilitation of Existing Buildings,” American Society of Civil Engineering, Reston, VA, 2017.

2. ACI Committee 369, “Standard Requirements for Seismic Evaluation and Retrofit of Existing Concrete Buildings (ACI 369.1-17),” American Concrete Institute, Farmington Hills, MI, 2017, 110 pp.

3. Los Angeles Tall Buildings Structural Design Council, “An Alternative Procedure for Seismic Analysis and Design of Tall Buildings Located in the Los Angeles Region,” Los Angeles, CA, 2017, pp. 56.

4. Applied Technology Council, “Guidelines for Nonlinear Structural Analysis for Design of Buildings, Part I – General, Part IIa – Steel Moment Frames, Part IIb – Reinforced Concrete Moment Frames,” U.S. Department of Commerce, April 2017.

5. Sokoli, D., “Fracture of High-Strength Bars in Concrete Frame Members under Earthquake Loads” PhD dissertation, The University of Texas at Austin, Austin, TX, 2018, 323 pp.

6. To, D. V., and Moehle, J. P., “Seismic Performance Characterization of Beams with High-Strength Reinforcement,” Charles Pankow Foundation, Haymarket, VA, 2017, 140 pp.

7. Ghannoum, W. M., Sokoli, D., Hogsett, G., Limantono, A., Suselo, A., Al-Tarafany, D., and Rodgers, S., “Acceptable Elongations and Low-Cycle Fatigue Performance for High-Strength Reinforcing Bars,” Charles Pankow Foundation, Haymarket, VA, Aug. 2019, 213 pp.

8. Sokoli, D.; Limantono, A.; and Ghannoum, W. M., “Special Moment Frames with High-Strength Reinforcement – Part 2: Columns,” ACI Structural Journal, V. 117, No. 2, Mar. 2020, pp. 253-265

9. To, D. V., and Moehle, J. P., “Special Moment Frames with High-Strength Reinforcement – Part 1: Beams,” ACI Structural Journal, V. 117, No. 2, Mar. 2020, pp. 239-252.

10. McKenna, F.; Fenves, G. L.; Scott, M. H.; and Jeremie, B., Open System for Earthquake Engineering Simulation, Open System for Earthquake Engineering Simulation (OpenSEES), University of California, Berkeley, Berkeley, CA, 2000.

11. LeBorgne, M. R., “Modeling the Post Shear Failure Behavior of Reinforced Concrete Columns,” PhD dissertation, The University of Texas at Austin, Austin, TX, May 2012.

12. Sokoli, D., and Ghannoum, W. M., “High-Strength Reinforcement in Columns under High Shear Stresses,” ACI Structural Journal, V. 113, No. 3, May-June 2016, pp. 605-614. doi: 10.14359/51688203

13. Sokoli, D.; Shekarchi, W.; Buenrostro, E.; and Ghannoum, W. M., “Advancing Behavioral Understanding and Damage Evaluation of Concrete Members Using High-Resolution Digital Image Correlation Data,” Earthquakes and Structures, V. 7, No. 5, 2014, pp. 609-626. doi: 10.12989/eas.2014.7.5.609

14. Rajaei, S.; Hogsett, G.; Chapagain, B.; Banjade, S.; and Ghannoum, W. M., “Vision-Based Large-Field Measurements of Bridge Deformations,” Journal of Bridge Engineering, V. 28, No. 11, 2023, p. 04023075. doi: 10.1061/JBENF2.BEENG-5973

15. Ghannoum, W. M.; Diaz, M.; Rajae, S.; Banjade, S.; Chapagain, B.; and Hogsett, G., “CIV - Civil Infrastructure Vision© v1.0: Bridge Calibration User Manual and Validation Manual,” Center for Transportation Research (CTR), FHWA/TX-21/0-6950-1, 2021, 85 pp.

16. Sokoli, D., “Seismic Performance of Concrete Columns Reinforced with High Strength Steel,” master’s thesis, The University of Texas at Austin, Austin, TX, 2014, 166 pp.

17. Coleman, J., and Spacone, E., “Localization Issues in Force-Based Frame Elements,” Journal of Structural Engineering, ASCE, V. 127, No. 11, 2001, pp. 1257-1265. doi: 10.1061/(ASCE)0733-9445(2001)127:11(1257)

18. Spacone, E.; Filippou, F. C.; and Taucer, F. F., “Fibre Beam-Column Model for Nonlinear Analysis of R/C Frames. I: Formulation,” Earthquake Engineering and Structural Dynamics, V. 25, No. 7, 1996, pp. 711-725. doi: 10.1002/(SICI)1096-9845(199607)25:73.0.CO;2-9

19. Neuenhofer, A., and Filippou, F. C., “Evaluation of Nonlinear Frame Finite-Element Models,” Journal of Structural Engineering, ASCE, V. 123, No. 7, 1997, pp. 958-966. doi: 10.1061/(ASCE)0733-9445(1997)123:7(958)

20. Scott, M. H., and Fenves, G. L., “Plastic Hinge Integration Methods for Force-Based Beam–Column Elements,” Journal of Structural Engineering, ASCE, V. 132, No. 2, 2006, pp. 244-252. doi: 10.1061/(ASCE)0733-9445(2006)132:2(244)

21. Addessi, D., and Ciampi, V., “A Regularized Force-Based Beam Element with a Damage-Plastic Section Constitutive Law,” International Journal for Numerical Methods in Engineering, V. 70, No. 5, 2007, pp. 610-629. doi: 10.1002/nme.1911

22. Limantono, A. A., “Modeling Strain Demands in Longitudinal Steel Bars of Concrete Columns,” master’s thesis, University of Texas at Austin, Austin, TX, 2016, 178 pp.

23. Kent, D. C., and Park, R., “Flexural Members with Confined Concrete,” Journal of the Structural Division, ASCE, V. 97, No. 7, 1971, pp. 1969-1990. doi: 10.1061/JSDEAG.0002957

24. Scott, M. H., and Hamutcuoglu, O. M., “Numerically Consistent Regularization of Force-Based Frame Elements,” International Journal for Numerical Methods in Engineering, V. 76, No. 10, 2008, pp. 1612-1631. doi: 10.1002/nme.2386

25. Popovics, S., “A Numerical Approach to the Complete Stress-Strain Curve of Concrete,” Cement and Concrete Research, V. 3, No. 5, 1973, pp. 583-599. doi: 10.1016/0008-8846(73)90096-3

26. Karsan, I. D., and Jirsa, J. O., “Behavior of Concrete under Compressive Loading,” Journal of the Structural Division, ASCE, V. 95, No. 12, 1969, pp. 2543-2564. doi: 10.1061/JSDEAG.0002424

27. Mander, J. B.; Priestley, M. J. N.; and Park, R., “Theoretical Stress-Strain Model for Confined Concrete,” Journal of Structural Engineering, ASCE, V. 114, No. 8, 1988, pp. 1804-1826. doi: 10.1061/(ASCE)0733-9445(1988)114:8(1804)

28. Qi, X., and Moehle, J. P., “Displacement Design Approach for Reinforced Concrete Structures Subjected to Earthquakes,” Earthquake Engineering Research Center, University of California, Berkeley, Berkeley, CA, UCB/EERC-91/02, Jan. 1991, 186 pp.

29. Menegotto, M., and Pinto, P.E., “Method of Analysis for Cyclically Loaded R.C. Frames Including Changes in Geometry and Non-Elastic Behavior of Elements Under Combined Normal Force and Bending,” Istituto di Scienza e Tecnica delle Costruzioni, University of Rome, Rome, Italy, Report 32, 1973, 13 pp.

30. ASTM A1035/A1035M-16b, “Standard Specification for Deformed and Plain, Low-Carbon, Chromium, Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016.

31. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

32. Sezen, H., and Moehle, J. P., “Shear Strength Model for Lightly Reinforced Concrete Columns,” Journal of Structural Engineering, ASCE, V. 130, No. 11, 2004, pp. 1692-1703. doi: 10.1061/(ASCE)0733-9445(2004)130:11(1692)

33. Ghannoum, W. M., and Moehle, J. P., “Shake-Table Tests of a Concrete Frame Sustaining Column Axial Failures,” ACI Structural Journal, V. 109, No. 3, May-June 2012, pp. 393-402.

34. Elwood, K. J., and Eberhard, M. O., “Effective Stiffness of Reinforced Concrete Columns,” ACI Structural Journal, V. 106, No. 4, July-Aug. 2009, pp. 476-484.

35. Kwon, J., “Strength, Stiffness, and Damage of Reinforced Concrete Buildings Subjected to Seismic Motions,” PhD dissertation, The University of Texas at Austin, Austin, TX, May 2016.

36. Park, R., and Paulay, T., Reinforced Concrete Structures, Wiley, New York, 1974

37. Macchi, G.; Pinto, P.E.; and Sanpaolesi, L., “Ductility Requirements for Reinforcement Under Eurocodes,” Structural Engineering International, V. 6, No. 4, 1996, pp. 249-254.

38. Aoyama, H., Design of Modern Highrise Reinforced Concrete Structures, Imperial College Press, London, UK, 2001.


ALSO AVAILABLE IN:

Electronic Structural Journal