Analytical Model of Concrete Cyclic Behavior in Compression

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analytical Model of Concrete Cyclic Behavior in Compression

Author(s): Sama Mohammed Saleem, Salman A. Alshamrani, and Hayder A. Rasheed

Publication: Materials Journal

Volume: 122

Issue: 1

Appears on pages(s): 31-38

Keywords: compression loading; cyclic loops; envelope curve; stressstrain curve

DOI: 10.14359/51744376

Date: 1/1/2025

Abstract:
The modeling of concrete constitutive relationships in cyclic compression has attracted a lot of research attention. In this study, a normalized envelope stress-strain curve made for concrete in uniaxial compression is mathematically derived. The compression loops are formulated using a bilinear unloading path followed by a linear reloading path based on thorough observations and calibrations of available experimental data. The proposed normalized model is calibrated against a set of experimental cyclic stressstrain data. This model is shown to yield robust results by proving it successful in capturing five other independent experimental cyclic stress-strain curves. This proposed model may prove valuable for the implementation and analysis of members subjected to cyclic loading in numerical finite element analysis.

Related References:

1. Wang, H. C.; Zhao, J.; Li, J.; Braithwaite, C. H.; and Zhang, Q. B., “Progressive Fracturing of Concrete under Biaxial Confinement and Repetitive Dynamic Loadings: From Damage to Catastrophic Failure,” International Journal of Impact Engineering, V. 165, July 2022, Article No. 104232. doi: 10.1016/j.ijimpeng.2022.104232

2. Keerthana, K., and Chandra Kishen, J. M., “Micromechanics of Fracture and Failure in Concrete under Monotonic and Fatigue Loadings,” Mechanics of Materials, V. 148, Sept. 2020, Article No. 103490. doi: 10.1016/j.mechmat.2020.103490

3. Kumar, B., and Ray, S., “An Analytical Approach for the Fracture Characterization of Concrete under Cyclic Loading,” Materials Today: Proceedings, 2023, (in press). doi: 10.1016/j.matpr.2023.04.075

4. Zhang, J.; Yu, Z.; Tang, Y.; Shen, J.; and Chen, H., “Fracture Properties of Concrete under Cyclic Loading,” Construction and Building Materials, V. 281, Apr. 2021, Article No. 122610. doi: 10.1016/j.conbuildmat.2021.122610

5. Monnamitheen Abdul Gafoor, A. H., and Dinkler, D., “A Macroscopic Gradient-Enhanced Damage Model for Deformation Behavior of Concrete under Cyclic Loadings,” Archive of Applied Mechanics, V. 90, No. 5, May 2020, pp. 1179-1199. doi: 10.1007/s00419-020-01669-4

6. Lu, J.; Zhu, K.; Tian, L.; and Guo, L., “Dynamic Compressive Strength of Concrete Damaged by Fatigue Loading and Freeze-Thaw Cycling,” Construction and Building Materials, V. 152, Oct. 2017, pp. 847-855. doi: 10.1016/j.conbuildmat.2017.07.046

7. Kunnath, S. K., and Chai, Y. H., “Cumulative Damage‐Based Inelastic Cyclic Demand Spectrum,” Earthquake Engineering & Structural Dynamics, V. 33, No. 4, Apr. 2004, pp. 499-520. doi: 10.1002/eqe.363

8. Xiao, J.-Q.; Ding, D.-X.; Jiang, F.-L.; and Xu, G., “Fatigue Damage Variable and Evolution of Rock Subjected to Cyclic Loading,” International Journal of Rock Mechanics and Mining Sciences, V. 47, No. 3, Apr. 2010, pp. 461-468. doi: 10.1016/j.ijrmms.2009.11.003

9. Isojeh, B.; El-Zeghayar, M.; and Vecchio, F. J., “Concrete Damage under Fatigue Loading in Uniaxial Compression,” ACI Materials Journal, V. 114, No. 2, Mar.-Apr. 2017, pp. 225-235. doi: 10.14359/51689477

10. Wang, C.; Wu, H.; and Li, C., “Hysteresis and Damping Properties of Steel and Polypropylene Fiber Reinforced Recycled Aggregate Concrete under Uniaxial Low-Cycle Loadings,” Construction and Building Materials, V. 319, Feb. 2022, Article No. 126191. doi: 10.1016/j.conbuildmat.2021.126191

11. Sinha, B. P.; Gerstle, K. H.; and Tulin, L. G., “Stress-Strain Relations for Concrete Under Cyclic Loading,” ACI Journal Proceedings, V. 61, No. 2, Feb. 1964, pp. 195-211.

12. Karsan, I. D., and Jirsa, J. O., “Behavior of Concrete Under Compressive Loadings,” Journal of the Structural Division, ASCE, V. 95, No. 12, Dec. 1969, pp. 2543-2564. doi: 10.1061/JSDEAG.0002424

13. Yankelevsky, D. Z., and Reinhardt, H. W., “Model for Cyclic Compressive Behavior of Concrete,” Journal of Structural Engineering, ASCE, V. 113, No. 2, Feb. 1987, pp. 228-240. doi: 10.1061/(ASCE)0733-9445(1987)113:2(228)

14. Bahn, B. Y., and Hsu, C.-T. T., “Stress-Strain Behavior of Concrete under Cyclic Loading,” ACI Materials Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 178-193.

15. Chang, G. A., and Mander, J. B., “Seismic Energy Based Fatigue Damage Analysis of Bridge Columns: Part I—Evaluation of Seismic Capacity,” Technical Report NCEER-94-0006, National Center for Earthquake Engineering Research, State University of New York at Buffalo, Buffalo, NY, Mar. 1994, 244 pp.

16. Mansour, M., and Hsu, T. T. C., “Behavior of Reinforced Concrete Elements under Cyclic Shear. II: Theoretical Model,” Journal of Structural Engineering, ASCE, V. 131, No. 1, Jan. 2005, pp. 54-65. doi: 10.1061/(ASCE)0733-9445(2005)131:1(54)

17. Palermo, D., and Vecchio, F. J., “Compression Field Modeling of Reinforced Concrete Subjected to Reversed Loading: Formulation,” ACI Structural Journal, V. 100, No. 5, Sept.-Oct. 2003, pp. 616-625.

18. Sima, J. F.; Roca, P.; and Molins, C., “Cyclic Constitutive Model for Concrete,” Engineering Structures, V. 30, No. 3, Mar. 2008, pp. 695-706. doi: 10.1016/j.engstruct.2007.05.005

19. Chen, X.; Xu, L.; and Bu, J., “Experimental Study and Constitutive Model on Complete Stress-Strain Relations of Plain Concrete in Uniaxial Cyclic Tension,” KSCE Journal of Civil Engineering, V. 21, No. 5, July 2017, pp. 1829-1835. doi: 10.1007/s12205-016-0802-0

20. Chen, E.-S., and Buyukozturk, O., “Constitutive Model for Concrete in Cyclic Compression,” Journal of Engineering Mechanics, ASCE, V. 111, No. 6, June 1985, pp. 797-814. doi: 10.1061/(ASCE)0733-9399(1985)111:6(797)

21. Aslani, F., and Jowkarmeimandi, R., “Stress–Strain Model for Concrete under Cyclic Loading,” Magazine of Concrete Research, V. 64, No. 8, Aug. 2012, pp. 673-685. doi: 10.1680/macr.11.00120

22. Castaldo, P.; Gino, D.; Bertagnoli, G.; and Mancini, G., “Resistance Model Uncertainty in Non-linear Finite Element Analyses of Cyclically Loaded Reinforced Concrete Systems,” Engineering Structures, V. 211, May 2020, Article No. 110496. doi: 10.1016/j.engstruct.2020.110496

23. El Yassari, S., and El Ghoulbzouri, A., “Numerical Simulation of Fiber-Reinforced Concrete under Cyclic Loading Using Extended Finite Element Method and Concrete Damaged Plasticity,” International Journal of Engineering, V. 36, No. 10, Oct. 2023, pp. 1815-1826. doi: 10.5829/IJE.2023.36.10A.08

24. Varma, R. K.; Barros, J. A. O.; and Sena-Cruz, J. M., “Numerical Model for CFRP Confined Concrete Elements Subject to Monotonic and Cyclic Loadings,” Composites Part B: Engineering, V. 40, No. 8, Dec. 2009, pp. 766-775. doi: 10.1016/j.compositesb.2009.05.005

25. Vecchio, F. J., “Towards Cyclic Load Modeling of Reinforced Concrete,” ACI Structural Journal, V. 96, No. 2, Mar.-Apr. 1999, pp. 193-202.

26. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

27. Tanigawa, Y., and Uchida, Y., “Hysteretic Characteristics of Concrete in the Domain of High Compressive Strain,” Proceedings, Annual Architectural Institute of Japan (AIJ) Convention, Tokyo, Japan, 1979, pp. 449-450.

28. Okamoto, S.; Shiomi, S.; and Yamabe, K., “Earthquake Resistance of Prestressed Concrete Structures,” Proceedings, Annual Architectural Institute of Japan (AIJ) Convention, Tokyo, Japan, 1976, pp. 1251-1252.

29. Xu, L.; Li, B.; Ding, X.; Chi, Y.; Li, C.; Huang, B.; and Shi, Y., “Experimental Investigation on Damage Behavior of Polypropylene Fiber Reinforced Concrete under Compression,” International Journal of Concrete Structures and Materials, V. 12, No. 1, Dec. 2018, Article No. 68. doi: 10.1186/s40069-018-0302-3