Abstract:
When used properly, product samples can inspire and motivate an owner or decision-maker to choose a construction team and its products. Effective samples can tell the story of the substrate being addressed, the systems as they will be installed, and the anticipated finished outcome of the proposed project. They can also demonstrate the team’s craftsmanship and attention to detail.