Advancing Structural Engineering at the Built Environment and Structural System Center of The Hashemite University

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Advancing Structural Engineering at the Built Environment and Structural System Center of The Hashemite University

Author(s): Ahmad Tarawneh and Ahmad Mhanna

Publication: Concrete International

Volume: 46

Issue: 12

Appears on pages(s): 58-61

Keywords: research, testing, concrete, project

DOI: 10.14359/51744355

Date: 12/1/2024

Abstract:
The Built Environment and Structural System Center (BESSC) at The Hashemite University in Zarqa, the Hashemite Kingdom of Jordan, is a beacon of progress in this field in the Middle East. Established with a vision to elevate structural engineering, concrete innovation, and educational processes, BESSC serves as a hub for structural and material testing and expert consultations.