Excessive Overdesign of Concrete Mixtures for Strength—Causes and Solutions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Excessive Overdesign of Concrete Mixtures for Strength—Causes and Solutions

Author(s): Luke M. Snell, Karthik H. Obla, and Nicholas J. Carino

Publication: Concrete International

Volume: 46

Issue: 11

Appears on pages(s): 49-55

Keywords: concrete, design, test, requirements

DOI: 10.14359/51743317

Date: 11/1/2024

Abstract:
Overdesigning concrete mixtures for compressive strength results in an increased carbon footprint due to much higher cementitious materials content and added construction costs. This article discusses some of the reasons why concrete mixtures are overdesigned and offers recommendations to avoid unnecessarily high overdesigns.

Related References:

1. ACI Committee 301, “Specifications for Concrete Construction (ACI SPEC-301-20),” American Concrete Institute, Farmington Hills, MI, 2020, 69 pp.

2. ACI Committee 318, “Building Code Requirements for Structural Concrete and Commentary (ACI CODE-318-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

3. Cook, J.E., “Research and Application of High-Strength Concrete Using Class C Fly Ash,” Concrete International, V. 4, No. 7, July 1982, pp. 72-80.

4. “A Cradle-to-Gate Life Cycle Assessment of Ready-Mixed Concrete Manufactured by NRMCA Members – Version 3.2,” Athena Sustainable Materials Institute, Ottawa, ON, Canada, 2022, 101 pp., https://www.nrmca.org/wp-content/uploads/2022/02/NRMCA_LCAReportV3-2_20220224.pdf.

5. ACI Committee 329, “Minimum Cementitious Materials Content in Specifications (ACI PRC-329.1T-18),” American Concrete Institute, Farmington Hills, MI, 2018, 4 pp.

6. ACI Committee 363, “Report on High-Strength Concrete (ACI PRC-363-10),” American Concrete Institute, Farmington Hills, MI, 2010, 65 pp.

7. ACI Committee E702, “Designing Concrete Structures: Evaluation of Concrete Cores Test Results According to ACI 318-19 (ACI E702.8-22),” American Concrete Institute, Farmington Hills, MI, 2022, 8 pp.

8. “Guide to Improving Specifications for Ready Mixed Concrete,” NRMCA Publication 2PE004-21, National Ready Mixed Concrete Association, Alexandria, VA, 2021, 37 pp., https://www.nrmca.org/wp-content/uploads/2020/10/GuideToSpecs.pdf.

9. ACI Committee 132, “Guide for Responsibility in Concrete Construction (ACI PRC-132-14),” American Concrete Institute, Farmington Hills, MI, 2014, 11 pp.

10. “Concrete Testing Adherence Collaboration,” Colorado Ready Mixed Concrete Association (CRMCA), Centennial, CO, https://www.concretetac.com/, accessed Apr. 12, 2024.

11. Obla, K.H.; Werner, O.R.; Hausfeld, J.L.; MacDonald, K.A.; Moody, G.D.; and Carino, N.J., “Who is Watching Out for the Cylinders?” Concrete International, V. 40, No. 8, Aug. 2018, pp. 28-35.

12. “Reliable Concrete Acceptance Testing for Improved Sustainability and Performance,” NRMCA Position Statement, National Ready Mixed Concrete Association, Alexandria, VA, 2024, 2 pp., https://www.nrmca.org/wp-content/uploads/NRMCA_Position_Statement.pdf.

13. ACI Committee 311, “Specification for Testing Ready-Mixed Concrete (ACI SPEC-311.6-18),” American Concrete Institute, Farmington Hills, MI, 2018, 5 pp.

14. “AIA MasterSpec: Section 033000 – Cast-in-Place Concrete,” American Institute of Architects, Washington, DC, 2023, 64 pp.

15. “In-Place Concrete Strength Evaluation—A Recommended Practice,” NRMCA Publication No. 133, National Ready Mixed Concrete Association, Alexandria, VA, 2011, 10 pp.

16. “Materials Manual,” Volume II, Section 9.2.6.3.1, revised July 2024, Florida Department of Transportation, Tallahassee, FL, https://fdotwww.blob.core.windows.net/sitefinity/docs/default-source/programmanagement/implemented/urlinspecs/july24/section92v2-724clnaede6fc2-255d-477f-8e3e-081b29cb864d.pdf?sfvrsn=4154e834_1.

17. ACI Committee 214, “Guide to Evaluation of Strength Test Results of Concrete (ACI PRC-214R-11) (Reapproved 2019),” American Concrete Institute, Farmington Hills, MI, 2011, 16 pp.