Title: Creep-Fatigue Interaction for Carbon Fiber-Reinforced Polymer-Prestressed Concrete Bridge Girders

Author(s): Yail J. Kim, Jun Wang, Woo-Tai Jung, Jae-Yoon Kang, and Jong-Sup Park

Publication: Structural Journal

Volume: 122

Issue: 2

Appears on pages(s): 113-128

Keywords: carbon fiber-reinforced polymer (CFRP); creep; fatigue; prestressed concrete; time-dependent behavior

DOI: 10.14359/51743304

Date: 3/1/2025

Abstract:
This paper presents the implications of creep-fatigue interactions for the long-term behavior of bulb-tee bridge girders prestressed with either steel strands or carbon fiber-reinforced polymer (CFRP) tendons. A large amount of weigh-in-motion data incorporating 194 million vehicles are classified to realistically represent live loads. Computational simulations are conducted as per the engagement of discrete autonomous entities in line with time- dependent material models. In general, the properties of CFRP tendons vary insignificantly over 100 years; however, the stress range of CFRP responds to fatigue cycles. Regarding prestress losses, the conventional method with initial material properties renders conservative predictions relative to refined approaches considering time-varying properties. The creep and fatigue effects alter the post-yield and post-cracking responses of steel- and CFRP-prestressed girders, respectively. From deformational capability standpoints, steel-prestressed girders are more vulnerable to fatigue in comparison with CFRP-prestressed ones. It is recommended that the fatigue truck and the compression limit of published specifications be updated to accommodate the ramifications of contemporary traffic loadings. Although the operational reliability of both girder types is satisfactory, CFRP-prestressed girders outperform their steel counterparts in terms of fatigue safety. Technical findings are integrated to propose design recommendations.

Related References:

1. FHWA, “Exploring Vehicle Size and Weight Solutions,” Report No. FHWA-HRT-09-004, Federal Highway Administration, Washington, DC, 2009.

2. FHWA, “Traffic Volume Trends,” Federal Highway Administration, Washington, DC, 2023.

3. AASHTO, “AASHTO LRFD Bridge Design Specifications, 9th Edition,” American Association of State Highway and Transportation Officials, Washington, DC, 2020.

4. Sun, B.; Xu, Y.-L.; Zhu, Q.; and Li, Z., “Auto-Adaptive Multiblock Cycle Jump Algorithm for Fatigue Damage Simulation of Long-Span Steel Bridges,” Fatigue and Fracture of Engineering Materials and Structures, V. 42, No. 4, 2018, pp. 919-928. doi: 10.1111/ffe.12960

5. Jiang, C.; Wu, C.; Cai, C. S.; and Xiong, W., “Fatigue Analysis of Stay Cables on the Long-Span Bridges under Combined Action of Traffic and Wind,” Engineering Structures, V. 207, 2020, p. 110212. doi: 10.1016/j.engstruct.2020.110212

6. Casas, J. R., and Crespo-Minguillon, C., “Probabilistic Response of Prestressed Concrete Bridges to Fatigue,” Engineering Structures, V. 20, No. 11, 1998, pp. 940-947. doi: 10.1016/S0141-0296(97)00187-9

7. Luo, Y.; Zheng, H.; Zhang, H.; and Liu, Y., “Fatigue Reliability Evaluation of Aging Prestressed Concrete Bridge Accounting for Stochastic Traffic Loading and Resistance Degradation,” Advances in Structural Engineering, V. 24, No. 13, 2021, pp. 3021-3029. doi: 10.1177/13694332211017995

8. AASHTO, 2018, “Guide Specifications for the Design of Concrete Bridge Beams Prestressed with Carbon Fiber-Reinforced Polymer (CFRP) Systems,” American Association of State Highway and Transportation Official, Washington, DC.

9. ACI Committee 440, “Prestressing Concrete Structures with FRP Tendons (ACI 440.4R-04) (Reapproved 2011),” American Concrete Institute, Farmington Hills, MI, 2004, 35 pp.

10. Grace, N. F.; Mohamed, M. E.; and Bebawy, M. R., “Evaluating Fatigue, Relaxation, and Creep Rupture of Carbon-Fiber Reinforced Polymer Strands for Highway Bridge Construction,” PCI Journal, V. 68, No. 3, 2023, pp. 36-61. doi: 10.15554/pcij68.3-01

11. Abdelrahman, A. A., and Rizkalla, S. H., “Serviceability of Concrete Beams Prestressed by Carbon Fiber-Reinforced-Plastic Bars,” ACI Structural Journal, V. 94, No. 4, July-Aug. 1997, pp. 447-454.

12. Poudel, P.; Belarbi, A.; Gencturk, B.; and Dawood, M., “Flexural Behavior of Full-Scale Carbon-Fiber-Reinforced Polymer Prestressed Concrete Beams,” PCI Journal, V. 67, No. 5, 2022, pp. 22-39. doi: 10.15554/pcij67.5-01

13. Saadatmanesh, H., and Tannous, F., “Relaxation, Creep, and Fatigue Behavior of Carbon Fiber-Reinforced Plastic Tendons,” ACI Materials Journal, V. 96, No. 2, Mar.-Apr. 1999, pp. 143-153.

14. Alam, P.; Mamalis, D.; Robert, C.; and Floreani, C., “The fatigue of Carbon Fibre Reinforced Plastics — A Review,” Composites Part B: Engineering, V. 166, 2019, pp. 555-579. doi: 10.1016/j.compositesb.2019.02.016

15. Abdallah, A. M.; Atadero, R. A.; and Ozbek, M. E., “A State-of-the-Art Review of Bridge Inspection Planning,” Journal of Bridge Engineering, ASCE, V. 27, No. 2, 2022, p. 03121001. doi: 10.1061/(ASCE)BE.1943-5592.0001812

16. CDOT, “Bridge Design Manual,” Colorado Department of Transportation, Denver, CO, 2022.

17. PCI, “Bridge Design Manual,” Precast/Prestressed Concrete Institute, Chicago, IL, 2014.

18. ACI Committee 209, “Guide for Modeling and Calculating Shrinkage and Creep in Hardened Concrete (ACI 209.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 44 pp.

19. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

20. Bažant, Z. P., “Prediction of Concrete Creep Effects Using Age-Adjusted Effective Modulus Method,” ACI Journal Proceedinsgs, V. 69, No. 4, Apr. 1972, pp. 212-219.

21. Tan, K. H., and Saha, M. K., “Long-Term Deflections of Reinforced Concrete Beams Externally Bonded with FRP System,” Journal of Composites for Construction, ASCE, V. 10, No. 6, 2006, pp. 474-482. doi: 10.1061/(ASCE)1090-0268(2006)10:6(474)

22. Hsu, T. T. C., “Fatigue of Plain Concrete,” ACI Journal Proceedinsgs, V. 78, No. 4, July-Aug. 1981, pp. 292-304.

23. fib, fib Model Code 2010, federation international du beton, Lausanne, Switzerland, 2010.

24. Harajli, M. H., and Naaman, A. E., “Static and Fatigue Tests on Partially Prestressed Beams,” Journal of Structural Engineering, ASCE, V. 111, No. 7, 1985, pp. 1602-1618. doi: 10.1061/(ASCE)0733-9445(1985)111:7(1602)

25. Irwin, C. A. K., “Static and Repetitive Loading Tests on Full Scale Prestressed Concrete Bridge Beams,” Report No. 802, Transport and Road Research Laboratory, Department of Transport, London, UK, 1977.

26. Han, J.; Song, Y.; Wang, L.; Song, S.; and Lei, B., “Steel Stress Redistribution and Fatigue Life Estimation of Partially Prestressed Concrete Beams under Fatigue Loading,” Advances in Structural Engineering, V. 17, No. 2, 2014, pp. 179-196. doi: 10.1260/1369-4332.17.2.179

27. Wang, C., and Zhang, J., “Experimental and Analytical Study on Residual Stiffness/Strength of CFRP Tendons Under Cyclic Loading,” Materials (Basel), V. 13, No. 24, 2020, p. 5653. doi: 10.3390/ma13245653

28. Elrefai, A.; West, J. S.; and Soudki, K., “Performance of CFRP Tendon-Anchor Assembly Under Fatigue loading,” Composite Structures, V. 80, No. 3, 2007, pp. 352-360. doi: 10.1016/j.compstruct.2006.05.023

29. Kim, J., and Song, J., “A Design Live Load Model for Long-Span Bridges Based on Traffic Data and Simulations,” Journal of Risk and Uncertainty in Engineering Systems, Part A: Civil Engineering, ASCE-ASME, V. 8, No. 4, 2022, p. 04022043

30. Kozikowski, M., “WIM Based Live Load Model for Bridge Reliability,” PhD dissertation, University of Nebraska Lincoln, Lincoln, NE, 2009.

31. Wilensky, U., and Rand, W., An Introduction to Agent-Based Modeling: Modeling Natural, Social, and Engineered Complex Systems with NetLogo, MIT Press, Cambridge, MA, 2015.

32. Feukeu, E. A., and Zuva, T., “DBSMA Approach for Congestion Mitigation in VANETs,” Procedia Computer Science, V. 109, 2017, pp. 42-49. doi: 10.1016/j.procs.2017.05.293

33. Wassef, W. G.; Kulicki, J. M.; Nassif, H.; Mertz, D.; and Nowak, A. S., Calibration of AASHTO LRFD Concrete Bridge Design Specifications for Serviceability, NCHRP 12-83, Transportation Research Board, Washington, DC, 2014.

34. Moses, F.; Schilling, C. G.; and Raju, K. S., Fatigue Evaluation Procedures for Steel Bridges, NCHRP-299, Transportation Research Board, Washington, DC, 1987.

35. CSiBridge, CSiBridge: Integrated 3-D Bridge Design Software, Computers & Structures, Inc., Berkeley, CA, 2011.

36. Saeed, Y. M., “Behavior of Prestressed Concrete Beams with CFRP Strands,” MS thesis, Portland State University, Portland, OR, 2016.

37. Braimah, A.; Green, M. F.; and Soudki, K. A., “Long-Term Behavior of CFRP Prestressed Concrete Beams,” PCI Journal, V. 48, No. 2, 2003, pp. 98-107. doi: 10.15554/pcij.03012003.98.107

38. Fang, Z., Jiang, R., Xiang, Y., and Liu, C., “Fatigue Behavior of Stirrup Free Reactive Powder Concrete Beams Prestressed with CFRP Tendons,” Journal of Composites for Construction, ASCE, V. 24, No. 4, 2020, p. 04020018. doi: 10.1061/(ASCE)CC.1943-5614.0001027

39. Liang, X.; Luo, L.; Hu, S.; and Li, Y., “Mapping the Knowledge Frontiers and Evolution of Decision Making Based on Agent-Based Modeling,” Knowledge-Based Systems, V. 250, 2022, p. 108982. doi: 10.1016/j.knosys.2022.108982

40. Kim, Y. J.; Wang, J.; Jung, W.-T.; Kang, J.-Y.; and Park, J.-S., “Failure-Mode-Dependent Behavior of CFRP-Prestressed Concrete Girders,” ACI Structural Journal, V. 120, No. 5, Sept. 2023, pp. 139-151.

41. Hassoun, M. N., and Al-Manaseer, A., Structural Concrete, John Wiley & Sons, Hoboken, NJ, 2008.

42. Yang, D.; Zhang, J.; Song, S.; Zhou, F.; and Wang, C., “Experimental Investigation on the Creep Property of Carbon Fiber Reinforced Polymer Tendons Under High Stress Levels,” Materials (Basel), V. 11, No. 11, 2018, p. 2273. doi: 10.3390/ma11112273

43. Peng, F.; Xue, W.; and Yu, T., “Cyclic Behavior of Polypropylene Fiber Reinforced Concrete Beams with Prestressed CFRP Tendons and Nonprestressed Steel Bars,” Engineering Structures, V. 275, 2023, p. 115201. doi: 10.1016/j.engstruct.2022.115201

44. Shah, S.; Swarts, S. E.; and Ouyang, C., Fracture Mechanics of Concrete, John Wiley & Sons, New York, NY, 1995.

45. Kim, Y. J., and Nickle, R. W., “Long-Term Multipliers and Deformability of Fiber-Reinforced Polymer Prestressed Concrete,” ACI Structural Journal, V. 115, No. 1, Jan. 2018, pp. 223-234. doi: 10.14359/51700988

46. Ustrzycka, A.; Mroz, Z.; Kowalewski, Z. L.; and Kucharski, S., “Analysis of Fatigue Crack Initiation in Cyclic Microplasticity Regime,” International Journal of Fatigue, V. 131, 2020, p. 105342. doi: 10.1016/j.ijfatigue.2019.105342

47. Tilley, R. J. D., Understanding Solids, Wiley, West Sussex, UK, 2013.

48. Yarnold, M. T., and Weidner, J. S., “Truck Platoon Impacts on Steel Girder Bridges,” Journal of Bridge Engineering, ASCE, V. 24, No. 7, 2019, p. 06019003. doi: 10.1061/(ASCE)BE.1943-5592.0001431

49. INDOT, “Fatigue of Older Bridges in Northern Indiana Due to Overweight and Oversized Loads,” Report No. FHWA/IN/JTRP-2005/16-2, SPR-2385, Division of Research, Indiana Department of Transportation, West Lafayette, IN, 2006.

50. Barker, M. G., and Barth, K. E., “Improved Serviceability Criteria for Steel Girder Bridges,” Journal of Bridge Engineering, ASCE, V. 18, No. 7, 2013, pp. 673-677. doi: 10.1061/(ASCE)BE.1943-5592.0000402

51. Nowak, A. S., and Collins, K. R., Reliability of Structures, CRC Press, Boca Raton, FL, 2013.

52. Singh, V. P.; Jain, S. K.; and Tyagi, A., Risk and Reliability Analysis, ASCE Press, Reston, VA, 2007.


ALSO AVAILABLE IN:

Electronic Structural Journal