Title: Meeting Specification Requirements with Low-Carbon Materials

Author(s): Stephanie Hampton

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/24/2024

Abstract:
As the concrete construction industry responds to the need to reduce greenhouse gas emissions (GHGs), low-carbon specifications for concrete construction are becoming increasingly prevalent. With this paradigm shift come new specifications, means and methods, documentation requirements, and changes in expectations and associated responsibilities. Meeting specification requirements (strength, workability, durability, etc.) with new low-carbon materials as Material Suppliers