Near-Surface-Mounted Flexural Strengthening of Existing Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Near-Surface-Mounted Flexural Strengthening of Existing Concrete Structures

Author(s): Joseph L. Yamin and Daniel T. Millman

Publication: Concrete International

Volume: 46

Issue: 10

Appears on pages(s): 55-58

Keywords: reinforcement, bridge, bond, design

DOI: 10.14359/51743271

Date: 10/1/2024

Abstract:
Near-surface-mounted (NSM) reinforcement can be used for strengthening of concrete members without extensive demolition of concrete sections. The article offers a historical review of this strengthening method and discusses its basic mechanics and design considerations, as well as projects where NSM was used for flexural strengthening of bridge elements.

Related References:

1. Asplund, S.O., “Strengthening Bridge Slabs with Grouted Reinforcement,” ACI Journal Proceedings, V. 45, No. 1, Jan. 1949, pp. 397-406.

2. ACI Committee 440, “Design and Construction of Externally Bonded Fiber-Reinforced Polymer (FRP) Systems for Strengthening Concrete Structures—Guide (ACI PRC-440.2-23),” American Concrete Institute, Farmington Hills, MI, 2023, 109 pp.

3. AASHTO NSMT-1, “Guide for Design and Construction of Near-Surface Mounted Titanium Alloy Bars for Strengthening Concrete Structures,” American Association of State and Highway Transportation Officials, Washington, DC, 2020, 48 pp.

4. Adkins, J., and George, W., “Titanium Finds a Home in Civil Engineering,” Concrete International, V. 39, No. 12, Dec. 2017, pp. 51-55.

5. “AASHTO LRFD Bridge Design Specifications,” eighth edition, American Association of State and Highway Transportation Officials, Washington, DC, 2017, 1762 pp.