Stress-Strain Response of BCSA Cement Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stress-Strain Response of BCSA Cement Concrete

Author(s): Victoria K. Sicaras

Publication: Concrete International

Volume: 46

Issue: 10

Appears on pages(s): 49-53

Keywords: hydraulic, cement, compression, research

DOI: 10.14359/51743263

Date: 10/1/2024

Abstract:
A 2-year research project funded by the ACI Foundation measured ultimate strain and stress behavior with controlled experiments to verify that the flexural capacity procedures in ACI 318-19(22) can work for concrete made with belite calcium sulfoaluminate (BCSA) cement. The results indicate that BCSA cement concrete behaves similarly to portland cement concrete in compression and has similar modulus of elasticity and compression strain characteristics.