Further Thoughts on "Tilt-Up Design Pitfalls"

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Further Thoughts on "Tilt-Up Design Pitfalls"

Author(s): Peter H. Bischoff

Publication: Concrete International

Volume: 46

Issue: 10

Appears on pages(s): 39-43

Keywords: wall, load, moment, deflection

DOI:

Date: 10/1/2024

Abstract:
The article discusses slender wall design at service loads with the new expression for the effective moment of inertia introduced into ACI 318-19(22), which now uses a reduced cracking moment for computing deflection. A recommendation is also made to provide a limiting condition for the axial wall load to avoid erroneous calculation of the factored moment by direct calculation.




  