408.1R-90: Suggested Development, Splice, and Standard Hook Provisions for Deformed Bars in Tension

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 408.1R-90: Suggested Development, Splice, and Standard Hook Provisions for Deformed Bars in Tension

Author(s):

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s): 3

Keywords: age; bond; building codes; development length; hooks; reinforced concrete; reinforcing steel; splices; structural design

DOI:

Date: 1/1/1990

Abstract:
This document presents recommendations for code provisions for development, splice length, and hooked anchorages for bars in tension. The recommendations explicitly consider cover, bar spacing, and transverse steel. There is no difference between development and splice length provisions, and hook design is independent of the development of straight bars.