Predicting Sorptivity via Surface Wettability: A Computer Vision Approach

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Predicting Sorptivity via Surface Wettability: A Computer Vision Approach

Author(s): Hossein Kabir

Publication: Web Session

Volume: ws_S24_Kabir.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/24/2024

Abstract:
The inherent ability of cementitious systems to absorb and transmit liquids through tiny capillary pores is commonly assessed using initial sorptivity, which serves as a crucial indicator of their long-term durability. However, the conventional method for determining sorptivity involves labor-intensive measurements that can take up to 6 hours, as it relies on continuous monitoring of specimen mass changes when exposed to water. In our study, using computer vision, we leverage the inherent surface-wetting properties of cementitious systems to swiftly estimate sorptivity, accomplishing this task in just a matter of minutes. Through a comprehensive analysis of 63 different paste systems featuring varying water-to-cement ratios (ranging from 0.4 to 0.8) and subjected to various curing periods (ranging from 1 to 7 days), we establish robust correlations (with adjusted R-squared values exceeding 0.9) between the initial sorptivity (measured over approximately 6 hours) and the dynamics of liquid drop spreading. This includes a contact angle measurement of around 0.5 seconds and a drop residence time of less than 10 minutes. These findings facilitate rapid and automated assessment of initial sorptivity and long-term durability of cementitious materials.