Title: Concrete Q&A: Further Discussion on Low-Carbon Concrete Mixtures

Author(s):

Publication: Concrete International

Volume: 46

Issue: 9

Appears on pages(s): 71-72

Keywords: low carbon, embodied carbon, embodied energy, global warming potential

DOI: 10.14359/51742221

Date: 9/1/2024

Abstract:
Understanding how to meet low-carbon concrete (LCC) mixture requirements is a challenge that many in the concrete industry now face. Part of the challenge is that the definition and reporting requirements for LCC vary widely by jurisdiction and specifying agency. Global warming potential limits, per mixture or per project requirements, and industry-average environmental product declarations have to be considered.

Related References:

1. “Concrete Q&A: Low-Carbon Concrete Mixtures,” Concrete International, V. 45, No. 11, Nov. 2023, pp. 109-112.

2. The Sustainable Concrete Guide—Applications, A.J. Schokker, ed., U.S. Green Concrete Council, Farmington Hills, MI, 2010, 177 pp.

3. Schokker, A., The Sustainable Concrete Guide—Strategies and Examples, U.S. Green Concrete Council, Farmington Hills, MI, 2009, 89 pp.

4. ACI Committee 130, “Report on the Role of Materials in Sustainable Concrete Construction (ACI 130R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 34 pp.

5. Simonen, K.; Rodriguez, B.X.; and De Wolf, C., “Benchmarking the Embodied Carbon of Buildings,” Technology|Architecture + Design, V. 1, No. 2, 2017, pp. 208-218.

6. “Product Category Rule for Environmental Product Declarations: PCR for Precast Concrete – UNCPC: 37550,” NSF International, Ann Arbor, MI, 2021, 40 pp.