ACI PRC-ITG-11-24: Statistical Techniques for Assessment of Existing Concrete Structures—Report

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI PRC-ITG-11-24: Statistical Techniques for Assessment of Existing Concrete Structures—Report

Author(s): Innovation Task Group 11

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 47

Keywords:

DOI:

Date: 8/22/2024

Abstract:
This report demonstrates how statistical techniques can be used in the assessment of concrete structures to evaluate their condition and reliability and to assess the relative merits of possible repair options. A Reliability Toolkit provides licensed design professionals with a summary of some statistical methods that are useful for structural assessment. The report also gives two detailed examples of assessments for structural concrete repair. Keywords: confidence level; data analysis; durability; material properties; mean load method; rehabilitation; reliability; sample size; testing.