Effect of Air-Entraining Agent on Rheology of Cement- Based Magnetorheological Pastes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Air-Entraining Agent on Rheology of Cement- Based Magnetorheological Pastes

Author(s): Junhyung Kim and Raissa Douglas Ferron

Publication: Materials Journal

Volume: 121

Issue: 5

Appears on pages(s): 3-12

Keywords: air-entraining agent (AEA); magnetorheological (MR) paste; rheology; small-amplitude oscillatory shear (SAOS); smart material; storage modulus.

DOI: 10.14359/51742113

Date: 9/1/2024

Abstract:
Embedding magnetic particles into cement paste produces a smart material in which the rheological properties of the resultant paste can be actively controlled through the use of magnetorheological (MR) principles. This research investigates the rheological behavior of cement-based MR pastes with and without air entrainment to gain a better understanding of the effects of air-entrained bubbles on MR cement pastes. Such information would be critical for the use of such MR pastes in three-dimensional (3-D) concrete printing applications. It is revealed that the incorporation of entrained air increases the MR response, and this effect is related to the bubble-bridge effect.

Related References:

ASTM C1738/C1738M-19, 2019, “Standard Practice for High-Shear Mixing of Hydraulic Cement Pastes,” ASTM International, West Conshohocken, PA, 3 pp.

Banfill, P. F. G., ed., 1991, Rheology of Fresh Cement and Concrete: Proceedings of an International Conference, Liverpool, 1990, first edition, CRC Press, London, UK, 373 pp.

Bos, F.; Wolfs, R.; Ahmed, Z.; and Salet, T., 2016, “Additive Manufacturing of Concrete in Construction: Potentials and Challenges of 3D Concrete Printing,” Virtual and Physical Prototyping, V. 11, No. 3, pp. 209-225. doi: 10.1080/17452759.2016.1209867

Clement, E., 1999, “Rheology of Granular Media,” Current Opinion in Colloid & Interface Science, V. 4, No. 4, Aug., pp. 294-299.

de Vicente, J.; Klingenberg, D. J.; and Hidalgo-Alvarez, R., 2011, “Magnetorheological Fluids: A Review,” Soft Matter, V. 7, No. 8, Apr., pp. 3701-3710. doi: 10.1039/c0sm01221a

Edmeades, R. M., and Hewlett, P. C., 1998, “Cement Admixtures,” Lea’s Chemistry of Cement and Concrete, fourth edition, P. C. Hewlett, ed., Butterworth-Heinemann, Oxford, UK, pp. 841-905.

Ferron, R. P.; Gregori, A.; Sun, Z.; and Shah, S. P., 2007, “Rheological Method to Evaluate Structural Buildup in Self-Consolidating Concrete Cement Pastes,” ACI Materials Journal, V. 104, No. 3, May-June, pp. 242-250.

Friederang, A. W., and Schlegel, R., 1999, “BASF Continues to Evolve Carbonyl Iron Powders,” Metal Powder Report, V. 54, No. 3, Mar., pp. 18-20.

Guo, Y.-Q.; Xie, W.-H.; and Jing, X., 2019, “Study on Structures Incorporated With MR Damping Material Based on PSO Algorithm,” Frontiers in Materials, V. 6, Mar., Article No. 37. doi: 10.3389/fmats.2019.00037

Jeyakumar, M.; Hamed, M.; and Shankar, S., 2011, “Rheology of Liquid Metals and Alloys,” Journal of Non-Newtonian Fluid Mechanics, V. 166, No. 14-15, Aug., pp. 831-838.

Kitazawa, K.; Ikezoe, Y.; Uetake, H.; and Hirota, N., 2001, “Magnetic Field Effects on Water, Air and Powders,” Physica B: Condensed Matter, V. 294-295, Jan., pp. 709-714.

Łaźniewska-Piekarczyk, B., 2013, “The Influence of Chemical Admixtures on Cement Hydration and Mixture Properties of Very High Performance Self-Compacting Concrete,” Construction and Building Materials, V. 49, Dec., pp. 643-662. doi: 10.1016/j.conbuildmat.2013.07.072

Nair, S. D., 2013, “Adaptive Performance of Cement-based Materials Using a Magnetorheological Approach,” PhD dissertation, The University of Texas at Austin, Austin, TX, 206 pp.

Nair, S. D., and Ferron, R. D., 2014, “Set-on-Demand Concrete,” Cement and Concrete Research, V. 57, Mar., pp. 13-27. doi: 10.1016/j.cemconres.2013.12.001

Nair, S. D., and Ferron, R. D., 2016, “Real Time Control of Fresh Cement Paste Stiffening: Smart Cement-Based Materials via a Magnetorheological Approach,” Rheologica Acta, V. 55, No. 7, July, pp. 571-579. doi: 10.1007/s00397-016-0923-x

NETZSCH, 2021, “NGB White Paper: A Basic Introduction to Rheology,” NETZSCH-Gerätebau GmbH, Selb, Germany, 16 pp.

Rahman, M. A., and Nehdi, M., 2003, “Effect of Geometry, Gap, and Surface Friction of Test Accessory on Measured Rheological Properties of Cement Paste,” ACI Materials Journal, V. 100, No. 4, July-Aug., pp. 331-339. doi: 10.14359/12672

Ramachandran, V. S.; Feldman, R. F.; and Beaudoin, J. J., 1981, Concrete Science: Treatise on Current Research, Heyden and Son Limited, London, UK, 448 pp.

Ranjan, P.; Balasubramaniam, R.; and Jain, V. K., 2017, “Analysis of Magnetorheological Fluid Behavior in Chemo-Mechanical Magnetorheological Finishing (CMMRF) Process,” Precision Engineering, V. 49, July, pp. 122-135. doi: 10.1016/j.precisioneng.2017.02.001

Science Kit Store, 2022, “Carbonyl Iron Powder, Zero Valent, High Purity Product Description,” MiniScience Company LLC, Clifton, NJ, https://sciencekitstore.com/carbonyl-iron-powder-zero-valent-high-purity/?sku=CIPMS-3LBS. (last accessed Aug. 15, 2024)

Shah, H. A.; Yuan, Q.; and Zuo, S., 2021, “Air Entrainment in Fresh Concrete and Its Effects on Hardened Concrete-A Review,” Construction and Building Materials, V. 274, Mar., Article No. 121835. doi: 10.1016/j.conbuildmat.2020.121835

Sika USA, 2023, “Product Data Sheet: Sika® AIR,” Version 02.04, Sika Corporation, Lyndhurst, NJ, 3 pp., https://usa.sika.com/content/dam/dms/us01/2/sika_air.pdf. (last accessed Aug. 15, 2024)

Struble, L. J., and Jiang, Q., 2004, “Effects of Air Entrainment on Rheology,” ACI Materials Journal, V. 101, No. 6, Nov.-Dec., pp. 448-456.

Szwabowski, J., and Łaźniewska-Piekarczyk, B., 2008, “The Increase of Air Content in SCC Mixes under the Influence of Carboxylate Superplasticizer,” Cement Wapno Beton, V. 13, No. 4, pp. 205-215.

Tattersall, G. H., and Banfill, P. F. G., 1983, The Rheology of Fresh Concrete, Pitman Books Limited, London, UK, 356 pp.

Yun, K.-K.; Choi, S.-Y.; and Yeon, J. H., 2015, “Effects of Admixtures on the Rheological Properties of High-Performance Wet-Mix Shotcrete Mixtures,” Construction and Building Materials, V. 78, Mar., pp. 194-202. doi: 10.1016/j.conbuildmat.2014.12.117

Zhang, X.; Zhang, H.; Gao, H.; He, Y.; and Jiang, M., 2019, “Effect of Bubble Feature Parameters on Rheological Properties of Fresh Concrete,” Construction and Building Materials, V. 196, Jan., pp. 245-255. doi: 10.1016/j.conbuildmat.2018.11.088


ALSO AVAILABLE IN:

Electronic Materials Journal