Artificial Neural Networks for Prediction of Bond Strength between UHPC and FRP Reinforcing Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Artificial Neural Networks for Prediction of Bond Strength between UHPC and FRP Reinforcing Bars

Author(s): Ali Alatify and Yail J. Kim

Publication: Symposium Paper

Volume: 363

Issue:

Appears on pages(s): 137-148

Keywords: artificial neural network; bond; fiber reinforced polymer (FRP); machine learning; modeling; ultra-high performance concrete (UHPC)

DOI: 10.14359/51742111

Date: 7/1/2024

Abstract:
This paper presents the prediction of bond strength between ultra-high performance concrete (UHPC) and fiber reinforced polymer (FRP) reinforcing bars using an artificial neuronal network (ANN) approach. A large amount of datasets, consisting of 183 test specimens, are collected from literature and an ANN model is trained and validated. The ANN model includes six variable inputs (bar diameter, concrete cover, embedment length, fiber content, concrete strength, and rebar strength) and one output parameter (bond strength). The model performs better than other models excerpted from existing design guidelines and previously published papers. Follow-up studies are expected to examine the individual effects of the predefined input parameters on the bond strength of UHPC interfaced with FRP rebars.




  