ASTM C1152/C1152M-04(2012), "Standard Test Method for Acid-Soluble Chloride in Mortar and Concrete."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM C1152/C1152M-04(2012), "Standard Test Method for Acid-Soluble Chloride in Mortar and Concrete."

Author(s):

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 12/15/2012

Abstract:
This test method provides procedures for the sampling and analysis of hydraulic-cement mortar or concrete for chloride that is acid soluble under the conditions of test. In most cases, acid-soluble chloride is equivalent to total chloride.