Title: ASTM A370-14, "Standard Test Methods and Definitions for Mechanical Testing of Steel Products."

Author(s):

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 5/15/2014

Abstract:
These test methods cover procedures and definitions for the mechanical testing of steels, stainless steels, and related alloys. The various mechanical tests herein described are used to determine properties required in the product specifications. Variations in testing methods are to be avoided, and standard methods of testing are to be followed to obtain reproducible and comparable results. In those cases in which the testing requirements for certain products are unique or at variance with these general procedures, the product specification testing requirements shall control.