Title: ASTM A616/A616M-96a, "Standard Specification for Rail-Steel Deformed and Plain Bars for Concrete Reinforcement," (withdrawn 1999).

Author(s):

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 1/1/1996

Abstract:
This specification covers deformed and plain rail-steel concrete-reinforcement bars. The standard sizes and dimensions of deformed bars and their number designations shall be those listed in Table 1.